LLDPE M500026T

Brevis descriptio:

SABIC Brand

LLDPE| Iniectio MI=50

In Saudi Arabia

 


  • Pretium :1000-1200 USD/MT
  • Portus:Huangpu / Ningbo / Shanghai / Qingdao
  • MOQ:1*40GP
  • CAS No::9002-88-4
  • HS Codicis;3901402090
  • Mercedem:TT/LC
  • Product Detail

    Descriptio

    M500026T est densitas linearis Low Polyethylene gradus cum angusto pondere hypothetico distributione aptae ad injectiones aptationum. Disposita est dare optimum fluxum proprietatum cum melioribus temperaturas duritiem, accentus rima resistentia et gloss.

    Typical Property Pretio

    POTESTAS VALUES typicus UNITS PROBATIO METHODS
    POLYMER POLYMER   
    Density 926 kg/m³ ASTM D1505
    Confluat O Rate (MFR)   
    at 190℃ and 2.16 kg 50 g/10 min ASTM D1238
    MACHINA   
    Flexurae Fortitudo 9 MPa ASTM D790
    Modulus flexilis (1% Secant) 200 MPa ASTM D790 A
    Izod Impact virtus 500 J/m ASTM D256
    Duritia (Sshore D) 50 - ASTM D2240
    ESCR (10% Igepal), F50 3 Hrs ASTM D1693B
    ESCR (100% Igepal), F50 6 Hrs ASTM D1693B
    Accentus distrahentes ad cede (50mm/min) 10 MPa ISO 527-2 1A
    Accentus distrahentes confractus (5mm/min) 12 MPa ISO 527-2 1A
    Contentio distrahens ad confractus (5mm/min) >100 % ISO 527-2 1A
    Scelerisque   
    Vicat molliens Point 88 ASTM D1525
    Bridness Temperature <-75 ASTM D746

    Processus Conditions

    Conditiones processus typicae pro M500026T sunt: ​​Ferocactus temperatus: 180 - 230°C Temperatus Mold: 15 -60 °C Iniectio pressionis: 600 - 1000 Bar.

    Salutem et incolumitatem considerationes et cautiones

    M500026T apta ad applicationem contactuum Cibus est. Detailed informationes providetur in adiunctis Salutis Materialis Datasheet et ad informationes specificas informationes petentes SABIC locali pro certificatorio. REPUDIUM: This product is not intented for and must not be used in anymedicamenta / medicamenta medicamenta.

    Repono et tractantem

    Polyethylenae resina eo modo condi debet, ne directa expositio ad solem et/vel calorem reiciatur. Tabularium etiam arescere debet ac potius 50°C non excedere. SABIC warantizare non daret condiciones repositionis malae quae ad qualitatem depravationis inducere possunt sicut color mutatio, malus odor et inadaequata effectio producti. Expedit ad PE resinae processus intra 6 menses post partum.